Bluing is FeO3 or rust with an extra oxygen molecule. This conversion happens as part of the chemical reaction to the rusting agent in the boiling tank. I'm not a chemist by any means, so I'm sure there's a lot more to it than that. But I think you can get the gist.


Rust bluing 1911Forum

Well, we have to be realistic about the ability to fill pits. Consider that a hair is approximately 50µm in diameter and that bluing adds only 2µm at a time. Assume that it takes 5 applications of rust bluing to build it up to 2µm, it would take a total of 125 rust blue applications to fill a pit the same diameter as a human hair!


Rust Bluing Brian M. Dudley

Pour 420ml of distilled water into the amber bottle Using the volume measure, pour 29ml of hydrochloric acid and 35ml of nitric acid into the jar Using the scale, measure out 13.3g of iron filings


My first attempt at rust bluing

Rust Bluing Tutorial - Turn any Steel Object Black With Household Materials Beyond Ballistics 9.45K subscribers Subscribe 3.7K Share 198K views 8 months ago This is the first of a 3 video.


My peculiar nature Quick rust bluing Back in black!

Rust blue recipe The chemical recipe used to rust blue has two requirements. Firstly it should allow a controlled and dense corrosion to occur. Any chemical that induces rusting, could potentially be used as the rust blue solution, see my article What blue solution to use.


Rust Bluing • Enough Gun

180,797 views DIY Rust Bluing Recipe:4 TBSP Peroxide1TBSP White Vinegar3/4 TSP Non-iodized SaltBoil in Distilled Wateremail: [email protected]: @357.magdadMusic:.


Rust Bluing American Bluing & Guns, LLC

Weigh 33.25 grams of hot water and put into a small container B (used to dilute the Sodium Nitrate, which resembles sugar). Weigh 11.25 grams of Sodium Nitrate and add to hot water in container B. Lastly, add container B (Sodium Nitrate/Water solution) to container A (Brownell's Classic Blue Rust). Seal and shake the solution.


Rust bluing.

Phosphate Solution To prepare the phosphate dipping solution, fill a tank with water until 6 inches below the maximum fill level. Add the phosphate, as directed by the supplier. Add more water until you reach the fill level. Heat the solution until it is between 179.6 degrees Fahrenheit and 190.4 degrees Fahrenheit.


Slow Rust Bluing HiPower Pistol Part 2 Slow Rust Bluing YouTube

First, I detail stripped the gun and bagged the small parts together with other parts of their operating group. I put the parts in the tupperware container and filled it with the vinegar. Almost immediately, bubbles started forming. I let it sit for 15 minutes at a time and then carded it briskly with the brush. Soaking in vinegar.


Rust bluing solution. 100oz. Летательные аппараты

A. Try any recipe for black finish on steel; after that you can use phosphating and then clearcoat it. You can use black phosphating too (combined with clearcoat).. I second John Gellatly's slow rust bluing formula, i.e., 3 parts nitric acid, 2 parts hydrochloric acid, as much iron as it will dissolve and after cessation of the reaction.


Not So Slow Rust Bluing YouTube

#2 · Nov 9, 2021 I just use the Brownells . It is expensive but goes a long ways . One bottle has done several guns & still have 1/2 left . It is a fun interesting process . So far I have done hot blue. all kinds of cold blue.. steam pipe rust & box rust blue . It all comes down to the prep work you put into it .


PICS ADDED Neidner Recipe Slow Rust Bluing, completed mfgr., avail in 4OZ lots

Rust Bluing: DIY Tips and Techniques One of the most durable metal finishes available, express rust bluing doesnt require a large investment in time or equipment to produce professional-looking results. By estaff - Published: August 20, 2013 2 Before the advent of modern production methods, firearms manufacturers did things "the old-fashioned way."


My Rust Blue Recipe Firearm Bluing

Rust bluing is a very old method that has long served to protect gun barrels, but it has been used on trigger guards, toplevers and other furniture as well.. caustic compounds are mixed into a water bath that is in turn heated to temperatures around 350° F. Different hot bluing salt recipes result in very different color tones (e.g., the.


PICS ADDED Neidner Recipe Slow Rust Bluing, completed mfgr., avail in 4OZ lots

"Rust" bluing and "fume" bluing: Results in the best rust and corrosion resistance. The oxidation of the metal forms magnetite (Fe3O4), which is the a black oxide of iron. Deciding whether to blue Decide if and how much of the gun needs to be reblued. For minor wear, a cold bluing kit may be all you need.


Quick rust bluing. Very well explained! Back to black, Rust, Black

Rust bluing is done by boiling the parts in pure water, removing them and swabbing them with a chemical that causes the parts to rust. The rust is "carded" off with degreased steel wool, then put back in the water. Each time the rust formed by the chemical is carded off, the blue color gets deeper.


slow rust bluing process part 1 YouTube

Although slow rust bluing got its name because it's slow, it's a very simple process. Watch along as Larry Potterfield, Founder and CEO of MidwayUSA rust blu.